Reparatur von Blattscheiben
Reparatur von Blattscheiben
Die integrierte Schaufelscheibe ist ein Schlüsselbestandteil der Flugtriebwerksteile, Die Spitze der Klinge verschleißt während des Gebrauchs leicht, und die Blattwurzelenden sind anfällig für Rissbildung, was zu Ausschuss führt. Durch den Einsatz der additiven Fertigungstechnologie zur Laserreparatur kann in kurzer Zeit die direkte Formung der gesamten Blattscheibe erreicht werden, kann ein großartiges Programm sein, um Kosten zu sparen und die Produktionseffizienz zu verbessern.
Hintergrund des Projekts
The current manufacturing method of integral impeller uses forging, which has high forging cost and long cycle time, and the forged integral impeller will also have some metallurgical defects. The laser direct forming of aero-engine integral impeller can reduce the cost and speed up the cycle. The aero-engine integral impeller is prone to tip wear, cracking and other defects during use. In most cases, they are simply scrapped because they cannot be repaired. The cost of a direct replacement of an aero-engine impeller is very expensive, and the cost of a new product is generally not less than one million.
The whole leaf disc laser remanufacturing repair in foreign countries have successful cases, by foreign technical barriers, China in the whole blade of the laser remanufacturing technology has few successful applications. daher, the development of the overall leaf disc laser remanufacturing technology is an urgent technical problem to be solved.
Projektbeispiel
The overall leaf disc substrate material and laser cladding material are TC17, GH4169G. The laser cladding metallographic inspection meets the inspection requirements, with appropriate layer thickness, good side molding, no metallurgical defects, and uniform organization.
TC17 transverse cladding sample
Longitudinal cladding specimen
After the mechanical performance samples pass the test, the unit cladding and sample cladding repair are carried out. Man-made defects and repair defects by laser melting grid. In order to ensure the repair after cladding, a certain thickness needs to be guaranteed, and the scanning path needs to be designed according to the shape of the blade.
Through the cladding test of the single element, the feasibility of the cladding, the stability of the process, the cladding effect of the single element blade, including deformation, and the presence or absence of defects were confirmed, and the machining allowance and deformation were confirmed through the repair after cladding and so on.
Single element notch cladding effect
Nach der Verkleidung, Bei der Inspektion liegt kein Mangel vor, und das Endergebnis entspricht dem Projektabnahmestandard.
TC17 sample blade cladding test
>>The overall blisk laser additive manufacturing repair project completed the following technical content, and all passed the assessment test
- 1、Research on laser cladding performance.
- 2、Conduct basic process development.
- 3、Design and development of tooling and equipment applicable to laser additive manufacturing of integral leaf discs
- 4、Research and development of additive manufacturing equipment and repair process technology applicable to the overall leaf disc.
- 5、Conduct repair test of unit part sample
- 6、To carry out repair test of the whole leaf disc.
- 7、Conduct mechanical property test, unit part and overall part repair test.